Ex vivo detection and characterization of remineralized carious dentin, by nanoindentation and single point Raman spectroscopy, after amalgam restoration
FI: 2,969
Tipo: Article
Artículo original/colaboración Artículo original
Año: 2017
Autores
Toledano, M; Osorio, E; Aguilera, FS; Cabello, I; Toledano-Osorio, M; Osorio, R
Revista
Título: JOURNAL OF RAMAN SPECTROSCOPY